| Analysis | Test Method | Unit | Limit |
|---|---|---|---|
| Density@25°C | ASTM D-70 or ISIRI 3872 | Kg/mᵌ | 1010/1070 |
| Penetration@25°C | ASTM D-5 or ISIRI 2950 | mm/10 | 60/70 |
| Softening Point | ASTM D-36 or ISIRI 3868 | °C | 46 min |
| Ductility@25°C | ASTM D-113 or ISIRI 3866 | cm | 100 min |
| Loss on Heating | ASTM D-6 or ISIRI 2957 | wt% | 0.8 max |
| Flash Point | ASTM D-92 or ISIRI 1175 | °C | 230 min |
| Solubility in CS₂ | ASTM D-4 or ISIRI 2953 | wt% | 99.5 min |
| Spot Test | AA S H O T 102 or ISIRI 2949 | Negative | Negative |
| Drop in Penetration After Heating | ASTM D-6 & D-5 | wt% | 20 max |